Resources

Articles

Castables Designed for Hot Weather

Aug 17, 2021, 13:25 PM by Trevor Hileman

RESCO’s “H” castables were specifically formulated for extended working time during summer or Hot weather conditions.  Resco has the ability to modify pumpable castable mixes to retard the set so that pumping in hot weather can proceed without the mix setting up in the pipe.

Effects of Hot Weather on Castables:

Hot weather temperatures can reduce working time and accelerate the setting of cement bonded castables. This can be a significant installation issue when considering pumping cement bonded castables in hot weather conditions. Hot weather conditions can heat the castable and mixing water along with the concrete pump equipment and pumping lines.

“H” castables have been formulated to have approximately 2 hours of working time at air temperatures up to 95°F (35°C) but also set within 24 hours after mixing.

It should be noted that “H” castables MUST NOT be used in cool or cold weather since the setting is extended. If “H” castables are used in cool or cold air temperature, there will be significantly delayed and MAY NOT SET HARD.

 

Brand Name

Description

Brand Number

QuikTurn 60PC-H

Low Cement, 60% Alumina, Pumpable

1561

QuikTurn AZS PC H

 

Low Cement, AZS Based, Pumpable

4423

QuikTurn 32-70 PC-H

Low Cement, 70% Alumina, Pumpable

7588

EZ Cubed 60 LQY (H)

Low Cement, 55% Alumina, Pumpable

8609

R-Max PC QT-H

Abrasion Resistant, 80% Alumina, Pumpable

7589

Unicrete 94H

Silica Free, High Purity Alumina Castable

3750

Vibrocast ASC Coarse H

Silica Free, Alumina Spinel Castable

4137

 

Load more comments